I-epoxy ye-alumina ye-ceramic ezaliswe ngamaso e-epoxy kunye nokumelana okubalaseleyo kwe-abrasion kwiimeko zenkonzo ezinzima

Inkcazelo emfutshane:

INxiba amaso e-ceramic adityanisiweyo azaliswe yi-epoxy yenziwe ngokusebenza okuphezulu okuxhathisayo kunye nokunxiba amasuntswana e-ceramic axhathisayo kunye ne-resin eguqukileyo eguqukileyo kunye ne-resin ekwaziyo ukumelana nobushushu.


Iinkcukacha zeMveliso

Iithegi zeMveliso

I-Wear compound ye-ceramic beads ezaliswe yi-epoxy yenziwe ngokusebenza okuphezulu ukumelana nokunxiba amasuntswana e-ceramic axhathisayo kunye ne-resin eguqukileyo eguqukileyo kunye ne-resin ekwazi ukumelana nobushushu.I-Ceramic beads i-compound yokunxiba isetyenziswa ngokubanzi ekulungiseni zonke iintlobo zeendawo zokunxiba kunye nokulungiselela i-community-resistant kunye ne-corrosion-resistant corrosion kumphezulu wazo zonke iintlobo zamalungu omatshini.Umzekelo: ukulungiswa kunye nokukhusela kwangaphambili kombhobho, i-elbow, impompo yodaka, impompo yesanti, i-centrifuge, ibhokisi yokupakisha, i-slurry ejikelezayo yempompo yomzimba, i-impeller, ubukhulu bentloko yenkqubo ye-desulfurization yesityalo, njl.

Iikhompawundi zokunxiba zikaYiho ziinkqubo ezizodwa ezinelungelo elilodwa lomenzi we-epoxy resin ezinedayimane eqinile

Amaso e-ceramic axhathisa ukutyibilika ngokutyibilika.

IZIKHOKELO ZOKUSETYENZISWA- Ukulungiswa komphezulu:

Ukulungiswa okufanelekileyo komphezulu kubaluleke kakhulu ekusebenzeni kwexesha elide le mveliso.Eyona kanye

iimfuno ziyahluka ngobunzima besicelo, ubomi benkonzo obulindelekileyo, kunye ne-substrate yokuqala

iimeko.

Ezona mpawu

• Ukunganciphisi

• Okugqwesileyo kwi-Wear Resistance

• Yandisa imijikelo yokuSebenza kweZixhobo

Iphepha leDatha lobuGcisa

Into Isalathiso
Umbala Mluvu (White Grain)
Ubuninzi (g/cm3) 2.0
Ubungakanani bobunzima (A:B) 2:1 okanye 1:1
Ixesha lokusebenza (min) 10~30 (inokwenziwa ngokwezifiso)
Ixesha elipheleleyo lokunyanga (h) 7
Ukuqina emva kokuqina (Unxweme D) 100.0
Amandla acinezelayo (Mpa) 111.0
Amandla okucheba (Mpa) 32
Ubushushu bokusebenza(℃) -20~80(Yenzelwe ubushushu obuphezulu)

Usetyenziso

1. iincinci ezincinci ze-ceramic compound zisetyenziswa ngokubanzi kwindawo apho kukho ukunxiba kunye nokugqwala, njengepompo ejikelezayo ye-slurry, i-sediment concentration yepompo, umbhobho, ukulungiswa ngokukhawuleza kwe-elbow, ukunyanga isantya.

2.Ukulungiswa kombhobho we-Desulfurization ukunxitywa kunye nokukrazula, kwaye ngoku umbhobho usetyenziswa ngokubanzi irabha evulziweyo, kodwa ukuxhathisa kwayo kunxitywa ngokubanzi, ukuchithwa kunye nokuthuthwa akulula, umjikelo wolondolozo olude.Ezi ngxaki zinokusonjululwa kusetyenziswa ikhompawundi yokunxiba i-ceramic.

3.ukulungiswa kombhobho wothuthu, ukufakwa kwemibhobho yogutyulo, isikrufu sokuhambisa kunye nezinye iindawo ezinomatshini.

IZIKHOKELO ZOKUSETYENZISWA- Ukulungiswa komphezulu

Ukulungiswa okufanelekileyo komphezulu kubaluleke kakhulu ekusebenzeni kwexesha elide le mveliso.Eyona kanye

iimfuno ziyahluka ngobunzima besicelo, ubomi benkonzo obulindelekileyo, kunye neMiqathango yokuqala ye-substrate.

1.Kuzo zonke izicelo ezithe nkqo okanye ngaphezulu, ukubopha i-welding yentsimbi eyandisiweyo yemesh kwi-substrate yentsimbi iyacetyiswa ngamandla phambi kokusetyenziswa kokuNxitywa.

Umdibaniso.

2. Coca, yome, kwaye igruzuke indawo yesicelo.Okukhona ngokucokisekileyo iqondo lokulungiswa komphezulu, kokukhona ukusebenza ngcono kwesicelo.Ukuba kunokwenzeka, kucetyiswa ukuba umphezulu wegrit uqhunyiswe kuMgangatho weMetal White Near (SSPC-SP10/NACE No.2).Ukusetyenziswa okuncinci, ukurhangqa umphezulu ngezixhobo zezandla kufanelekile.

Ukuxuba

1. Linganisa iinxalenye ezi-2 ze-resin ukuya kwi-1 inxalenye yokuqina ngomthamo okanye ubunzima kwindawo yokuxuba ecocekileyo neyomileyo.

kwaye uxube kunye de ufane ngombala.

Preheat intlaka ukuya kuphela malunga ne-21℃/90℉ kodwa ingagqithi kwi-37℃/100℉ .

2.Kwangoko emva kokuba i-abrasive

ukuqhushumba, hlikihla umaleko obhityileyo wezinto phezu komhlaba ukuze "umanzi" ukuze unamathele kakuhle.

Ukusebenza

1.Faka izinto ezixutywe ngokupheleleyo kwindawo elungiselelwe.2.Ekuqaleni sebenzisa izinto eziphathekayo kwinqanaba elincinci kakhulu

"ukumanzisa" ngaphandle kwaye uphephe ukubanjiswa komoya.3.Kwi-25℃/77℉, ixesha lokusebenza yimizuzu engama-30.

Ukusebenza kunye nokuqinisa ixesha kuxhomekeke kwiqondo lokushisa kunye nobunzima;iqondo lobushushu liphezulu, likhulu

ubunzima, kokukhona uqina ngokukhawuleza .4.Ixesha lokunyanga elisebenzayo ziiyure ezisi-7 ku-25℃/77℉.5.LUMKO!Sebenzisa

evunyiweyo, enoxinzelelo olulungileyo, isiphefumlo-moya esinikezelweyo xa uwelda okanye ukusika itotshi kufutshane nenyanga

ikhompawundi.Sebenzisa izixhobo zokuphefumla ezivunyiweyo xa utshisa, ukuwelda, okanye ukusika itotshi

ngaphakathi kufutshane nenkomponi enyangisiweyo.Sebenzisa isiphefumli esivunyiweyo sothuli kunye nenkungu xa usila okanye

umatshini wanyanga ikhompawundi.

MUSA ukusebenzisa amadangatye avulekileyo kwikhompawundi.Jonga ezinye izilumkiso kwiphepha leDatha loKhuseleko lweMathiriyeli.

IPACEJI & UKUGCINWA

10kg/Seti, A:B=1:1 okanye A:B=1:2

1. Gcina kwindawo epholileyo kunye neyomoya, ixesha lokugcina iminyaka emi-2.Emva komhla wokuphelelwa yisikhathi, ukuba i-viscosity ifanelekile, ingasetyenziselwa ngokuqhubekayo ngaphandle kokuchaphazela umphumo wokugqibela.

2. Le mveliso ayinabungozi kwaye inokuthuthwa njengekhemikhali jikelele.